Testing Erasteel MagnaCut (vs Crucible Original)

Crucible, Niagara, Erasteel, and MagnaCut In case you haven’t been following steel news, Crucible Steel went through a bankruptcy and no longer exists. I interviewed Bob Shabala of Niagara Specialty Metals about this transition several months ago. Niagara is the company that purchased ingots from Crucible and would hot roll, anneal, and distribute them to … Continue reading Testing Erasteel MagnaCut (vs Crucible Original)