Heat Treating and Processing, Nitrogen-alloyed, Toughness

Nitro-V – Its Properties and How to Heat Treat It

Thanks to Brad Ettinger, James Henley, and Edgar Candela for becoming Knife Steel Nerds Patreon supporters!

Nitro-V Steel

Nitro-V is a stainless steel sold by New Jersey Steel Baron which was first released in 2017 [1]. The steel was designed and produced in collaboration with Buderus Steel as a version of Uddeholm AEB-L modified with nitrogen and vanadium. Another obvious comparison is with 14C28N which was designed as a version of 13C26 modified for improved corrosion resistance. 13C26 is nearly identical to AEB-L but produced by Sandvik. You can read more about the history of AEB-L, 13C26, and 14C28N in this article. read more