Does Damascus Outperform Super Steels? Testing Different Combinations

It’s been a while since I posted a full article, so there are a bunch of new Patreon supporters. Thanks to our new supporters Jack Hilton, David Heleander, KevinP, huck, Dd, C, Brian Fencil, Rick Steele, Leon Rodak, Kendal Thomas, The Madman, Michael Kelly, Allen Thomas, Jim Pickard, Linqian Chen, Matt Masuda, Nick Dunham, Fikes Lee, Timothy Becker, jmasinter, MakaBones, Will from Maine, and Charles. Please go to Patreon.com/KnifeSteelNerds if you want to be a supporter. Damascus is very expensive and this is one of the priciest studies I have ever done for Knife Steel Nerds. I spent several months and about $10,000 to do the following study. Without reservation, I can say this is the biggest study on the performance of pattern-welded Damascus that has ever been performed. Your support means we can do more studies on knife steel that would be unrealistically expensive otherwise. read more