If you would like to support metallurgy research like this, please come join us at Patreon.com/KnifeSteelNerds. You get to see articles and videos early and join our community.
Video
Here is the video version of the following information:
If you would like to support metallurgy research like this, please come join us at Patreon.com/KnifeSteelNerds. You get to see articles and videos early and join our community.
Video
Here is the video version of the following information:
My steel research is supported through Patreon. Patreon supporters saw the news on Pop’s ProCut before anyone else. There is currently an article about the upcoming MagnaMax only available on Patreon.
Thanks to my Patreon supporters for supporting knife steel research. Patreon supporters saw this interview a couple of days ago. You can see the latest results of my testing early if you join at Patreon.com/KnifeSteelNerds
Still working on getting an update to everyone about the status of knife steel after Crucible’s bankruptcy and the sale of many of the assets to Erasteel. Still more i’s to dot and t’s to cross.
Patreon
Thank you Patreon supporters! Thanks to you we can do all the experiments that are in this article. If you want to support knife steel research come join us at Patreon.com/KnifeSteelNerds.
Video
Here is the video version of the following information:
Atlantic 33 Steel
There are a few places to purchase this Atlantic 33 “non-tempering” steel so I have been getting questions about it over the past couple years. The information is pretty scant and the descriptions are mysterious and confusing to anyone who knows steel [1]. In the advertising it says things like: “Drawing of temper to suit different requirements is unnecessary and completely eliminated.” Also there is no composition listed and the heat treating instructions are very barebones. “Suitable hardness is obtained by merely heating the tool and quenching it in water.” And, “May be heated to almost a melting heat without danger of distortion.” It basically just says to heat treat it however you feel like and skip the tempering. If it’s true that it doesn’t matter how you heat treat that is great, but otherwise it would be nice to know how to best heat treat the steel.
Patreon
Several new experiments were done to support this article. I am able to do these experiments thanks to the contributions of Patreon supporters. If you would like to support knife steel research visit Patreon.com/KnifeSteelNerds
Join the Knife Steel Nerds Patreon if you want my next update on the Crucible situation as soon as we know what happens with the bankruptcy sale.
Video
YouTube video for the following information:
The Current Production Path for MagnaCut and CPM Steels
If you want to support knife steel research, come join us at Patreon.com/KnifeSteelNerds. You get articles and videos before everyone else!
If you’re looking for Knife Steel Nerds Christmas gifts, some good choices are the book Knife Engineering, the book The Story of Knife Steel, and the Buck knife model 501 “The Larrin.”
Patreon
Thanks to my supporters on Patreon.com/KnifeSteelNerds. Thanks to your support we can do studies like this. Come join us on Patreon if you want support knife steel research too.
Video
I also have a video covering this same material: