How to Heat Treat MagnaMax Steel

Wide Release Date for MagnaMax for Small Knifemakers

MagnaMax will be on sale May 1st, 2026 at 9am on Niagara Specialty Metals’ online store: https://nsm-ny.com/shop/

You can create an account beforehand so that you are ready to buy once the steel goes live. We made the following commercial to get pumped for the release: read more