Thanks to my Patreon supporters for supporting knife steel research. Patreon supporters saw this interview a couple of days ago. You can see the latest results of my testing early if you join at Patreon.com/KnifeSteelNerds
CPM-3V – Still the Best High Toughness Steel
Still working on getting an update to everyone about the status of knife steel after Crucible’s bankruptcy and the sale of many of the assets to Erasteel. Still more i’s to dot and t’s to cross.
Factory vs Custom Heat Treating of Knives
Patreon
Thank you Patreon supporters! Thanks to you we can do all the experiments that are in this article. If you want to support knife steel research come join us at Patreon.com/KnifeSteelNerds.
Video
Here is the video version of the following information:
What is Atlantic 33 Non-Tempering Steel?
Atlantic 33 Steel
There are a few places to purchase this Atlantic 33 “non-tempering” steel so I have been getting questions about it over the past couple years. The information is pretty scant and the descriptions are mysterious and confusing to anyone who knows steel [1]. In the advertising it says things like: “Drawing of temper to suit different requirements is unnecessary and completely eliminated.” Also there is no composition listed and the heat treating instructions are very barebones. “Suitable hardness is obtained by merely heating the tool and quenching it in water.” And, “May be heated to almost a melting heat without danger of distortion.” It basically just says to heat treat it however you feel like and skip the tempering. If it’s true that it doesn’t matter how you heat treat that is great, but otherwise it would be nice to know how to best heat treat the steel.
Is 1084-15N20 the Best Pattern Welded Damascus?
Patreon
Several new experiments were done to support this article. I am able to do these experiments thanks to the contributions of Patreon supporters. If you would like to support knife steel research visit Patreon.com/KnifeSteelNerds
Crucible Steel is Bankrupt! What is Next for MagnaCut?
Join the Knife Steel Nerds Patreon if you want my next update on the Crucible situation as soon as we know what happens with the bankruptcy sale.
Video
YouTube video for the following information:
The Current Production Path for MagnaCut and CPM Steels
Can Artificial Intelligence Design a New Knife Steel?
If you want to support knife steel research, come join us at Patreon.com/KnifeSteelNerds. You get articles and videos before everyone else!
If you’re looking for Knife Steel Nerds Christmas gifts, some good choices are the book Knife Engineering, the book The Story of Knife Steel, and the Buck knife model 501 “The Larrin.”
Testing Cold Forged 52100 Knife Steel
Patreon
Thanks to my supporters on Patreon.com/KnifeSteelNerds. Thanks to your support we can do studies like this. Come join us on Patreon if you want support knife steel research too.
Video
I also have a video covering this same material:
Coatings vs Foil – Heat Treating Steel
Thank You Patreon
Thanks to my Patreon supporters I was able to buy all of the coatings to test for this article. If you want to support more knife steel research come join us at Patreon.com/KnifeSteelNerds
Introduction to Knife Steel Heat Treating from a Metallurgist
Join the Knife Steel Nerds Patreon if you want to support knife steel research and get articles and videos early. Or go for the “Ultimate” tier and get a Knife Steel Nerds mug!
Intro
I have many articles about all of the nitty gritty details of heat treating and the metallurgy behind every step. However, there may be some cases where knifemakers are afraid of all of the terminology and science and think heat treating is too complicated for them. When it comes down to it, the steps of heat treating are not particularly difficult. When you follow a recipe for how to make cookies you don’t need to know the science behind every step, but following them will still get you cookies at the end. An expert would know what went wrong if your cookies were too crunchy, too puffy, spread out too much, etc. And how to modify the recipe to change the flavor and texture of the cookies. However for most of us we will just follow the recipe. You can do the same thing with heat treating knife steel! So for this article I will tell you how to follow a datasheet. I will include some links to articles with more information about what happens in each step, but you can get to those when you are ready. Another great place to learn more about heat treating is my book Knife Engineering: Steel, Heat Treating, and Geometry.