Austenitic Stainless, Cold Forging, Corrosion Resistance

H2 Steel – H1 the sequel

Background

A recent Spyderco Byte has announced a replacement for H1 steel – H2. H1 is known for being a very high corrosion resistance steel used primarily in Spyderco’s Salt line of knives. I have a previous article about the design of H1 and how it “works” which you can read here. I am somewhat tempted to re-write large chunks of that article here because H1 is one of the most misunderstood knife steels but I am going to try to hit a few of the highlights without much explanation and I hope you will read the earlier article to understand what I am referring to: read more

Austenitic Stainless, Corrosion Resistance, History - Articles - Books, Steel and Knife Properties

H1 Steel – How it Works

Thanks to Guns N’ Loaded for becoming a Knife Steel Nerds Patreon supporter!

Austenitic Stainless Steels

At its most basic, H1 is an austenitic stainless steel. Austenitic stainless steels are about as old as stainless steel itself, being developed by German metallurgists in the approximate time period of 1909-1912. They worked on 18% Cr, 8% Ni steels which are quite similar to common austenitic stainless steels like 301, 302, and 304. read more