Category: Damascus
Making ProCut Damascus with Devin Thomas
We traveled to Nevada to visit my dad, Devin Thomas, and make some Damascus with Pop’s ProCut. Along the way we saw some sites around my hometown and my wife tries to prove that her town is better.
Pop’s ProCut – A New Carbon Steel for Knives
My steel research is supported through Patreon. Patreon supporters saw the news on Pop’s ProCut before anyone else. There is currently an article about the upcoming MagnaMax only available on Patreon.
Is 1084-15N20 the Best Pattern Welded Damascus?
Patreon
Several new experiments were done to support this article. I am able to do these experiments thanks to the contributions of Patreon supporters. If you would like to support knife steel research visit Patreon.com/KnifeSteelNerds
Wootz – The True Damascus Steel?
Thanks to Spencer Sandison for providing the Wootz steel for this new study! Thanks to Shawn Houston for performing the microscopy. And thanks to the Knife Steel Nerds Patreon supporters who allow me to do these studies through providing funds for all the experiments. All Patreon dollars go towards knife steel experiments.
Damasteel Heat Treatment and Properties
Thanks to the new Knife Steel Nerds Patreon supporters! The newly performed research in this article is all paid for through Patreon funds, such as the purchase of expensive Damasteel. Patreon money is only used for knife steel research. Sara Rempelos, Theo N, Christopher Kuehl, Dirk Hoogenbosch, Nick, nats spawnee, Krisztián Szegi, Todd Ellner, Seth V, Jonathan Graham, Ben Secrist, Drew Certain, Scott Armstuts, Ronald Justin Agee, Jim Darnall, Chris G, Farrell K., Bill Behnke, Paige, Luis Hernandez, clockworkfish, Barry Gordon, KarRawr, Ming Lin, Theodore Loach, Matt Bobchin, Flo, J.T. Pouland, Mark Watt, 愷麒 王, and Nickolay Matershev.
Does Damascus Outperform Super Steels? Testing Different Combinations
It’s been a while since I posted a full article, so there are a bunch of new Patreon supporters. Thanks to our new supporters Jack Hilton, David Heleander, KevinP, huck, Dd, C, Brian Fencil, Rick Steele, Leon Rodak, Kendal Thomas, The Madman, Michael Kelly, Allen Thomas, Jim Pickard, Linqian Chen, Matt Masuda, Nick Dunham, Fikes Lee, Timothy Becker, jmasinter, MakaBones, Will from Maine, and Charles. Please go to Patreon.com/KnifeSteelNerds if you want to be a supporter. Damascus is very expensive and this is one of the priciest studies I have ever done for Knife Steel Nerds. I spent several months and about $10,000 to do the following study. Without reservation, I can say this is the biggest study on the performance of pattern-welded Damascus that has ever been performed. Your support means we can do more studies on knife steel that would be unrealistically expensive otherwise.
The History of Powder Metals in Damascus Steel
Gratitude
Thanks to cbw, Doug Siddens, Nick Dunham, and Robert Martin for becoming Knife Steel Nerds Patreon supporters!
I interviewed several knifemakers for this article. Thanks to Ed Schempp, Hank Knickmeyer, Steve Schwarzer, Rick Dunkerley, Jim Batson, Shane Taylor, Jeff Carlisle, Kelly Cupples, Daryl Meier, John Davis, Matt Diskin, Wade Colter, Barry Gallagher, Howard Clark, Bob Kramer, and Devin Thomas for talking to me.
New Steel Analysis – Damasteel N11X and Damacore DC18N
Thanks to Bob Kramer, Jason Stone, Jeff Freeman, Austin Nader, Mark McKinley, and The_Iron_Joe for becoming Knife Steel Nerds Patreon supporters! We now have over 50 patrons!
N11X and Damacore DC18N
Last month I released an article about nitrogen-alloyed knife steels. After I posted the article I was informed about a new Damasteel product that includes a nitrogen-alloyed stainless steel as the core in a san-mai damascus steel product. At the time there was no information on the core steel other than its name: Damacore DC18N refers to a product with a core of “N11X” nitrogen steel and has san-mai damascus sides of RWL34 and PMC27 (their standard damascus mix without a core steel). Damasteel has recently released a datasheet for the new product which has provided more information: http://damasteel.se/wp-content/uploads/2018/06/Data-Sheet-Martensitic-Damacore-Final-Version.pdf
Five Myths About Damascus Steel
Knife Steel Nerds coffee mugs have been shipped to all current “Ultimate Steel Nerd” Patreon supporters.
What is Damascus Steel?
There are two major steel types that are called Damascus:
1. Crucible, or Wootz, steel was first produced in India and Central Asia and produced into swords anciently from at least the 3rd century AD [1]. It is made by producing small ingots of high carbon steel that are then forged and thermal cycled in a specific manner to lead to carbide bands that produce the final pattern when the steel is etched [2][3]: