Hardenability, History - Articles - Books

O1 Steel – History, Properties, and How to Heat Treat

Thanks to Johnny Ngo and ALtheSciencePal for becoming Knife Steel Nerds Patreon supporters!

O1 Steel History

O1 steel was developed in 1905 by Halcomb steel which was acquired by Crucible Steel a few years later [1][2]. However, the history is a bit more interesting than that. In 1876 a large Sheffield steel company, Sanderson Brothers, purchased Sweet’s Manufacturing Company’s Geddes Steel Works in Syracuse New York. American tariffs had led to a large reduction in exported steel from Sheffield, and steel output from the USA had also greatly increased to match. So several English steel companies setup production facilities in the US, including Sanderson Brothers. Sanderson Brothers was a very old Sheffield steel company, founded in 1776. Tool Steel development began to explode starting in about 1900 due to the recent discovery of “high speed steel” which you can read about here: The History of the First Tool Steel. The year 1900 was doubly significant because in that year there was a major consolidation of 13 of the major steel plants which used “crucible” steel production methods, accounting for 95% of the crucible steel production in the United States. read more

Damascus, Powder Metallurgy

The History of Powder Metals in Damascus Steel

Gratitude

Thanks to cbw, Doug Siddens, Nick Dunham, and Robert Martin for becoming Knife Steel Nerds Patreon supporters!

I interviewed several knifemakers for this article. Thanks to Ed Schempp, Hank Knickmeyer, Steve Schwarzer, Rick Dunkerley, Jim Batson, Shane Taylor, Jeff Carlisle, Kelly Cupples, Daryl Meier, John Davis, Matt Diskin, Wade Colter, Barry Gallagher, Howard Clark, Bob Kramer, and Devin Thomas for talking to me. read more

History - Articles - Books, Toughness

How to Heat Treat 26C3 Steel

Thanks to Gene Boyd and Dan Bidinger for becoming Knife Steel Nerds Patreon supporters!

26C3 Steel

26C3 steel is produced by Uddeholmstrip (part of Voestalpine Precision Strip) as a razor and scalpel steel. This steel is also known as 1.2002 using the German designation. I don’t know much about the history of the steel but the marketing literature says, “voestalpine Precision Strip AB has long experience and were the pioneers of both the high carbon (UHB 26C3) and the martensitic stainless steel (UHB AEB-L) razor strip grades” [1]. In the 1927 patent for AEB-H [2], reference is made to “the purest Swedish carbon steel with ‘1.05% C and 0.4% Mn'” and in a 1970 patent for a razor blade steel there is a reference to UHB 26C (the 3 is not on the end) which has the same approximate composition as the current 26C3 [3]. So I think there was probably some evolution of the composition despite the claims of the marketing material. The composition of 26C3 is shown below: read more

Corrosion Resistance, Edge Retention, Edge Stability, Steel and Knife Properties, Toughness

How to Design Knives that Do Not Fail

Thanks to Tom Krein, Joshua Goldstein, Matthew Maola, Edo Vernoschi, Nils Anderssen, and Cedric & Ada for becoming Knife Steel Nerds Patreon supporters!

Failure Modes

A common engineering technique is to evaluate designs based on how they failed, or may fail. Failure modes are identified and the designs are modified to prevent those failures. These ideas are simple in concept but it is surprising how easy it can be to miss the forest for the trees. In terms of predicting failure modes in some cases it is easy and in some it is difficult. You would expect a large chopping knife to require heavier edge geometry to prevent chipping and rolling, or a seawater diving knife to require high rust resistance. Other times failure modes are identified through testing of the knife or by returns from customers. Whatever the source of the failure, there are usually relatively simple methods for fixing each one, though the trade-offs for doing so may not be desirable. read more

History - Articles - Books

XHP Steel – History and Properties

Thanks to John Bates, Kenny Lazarus, Robert Abel, and Matt Danielson for becoming Knife Steel Nerds Patreon supporters! I have some exclusive Patreon supporter content this week. Pete of the Cedric and Ada Youtube channel posted this past week a video summarizing his rope cut tests on 14 Spyderco Mule knives in different steels. This is a fun test because all of the knives are nearly identical and only the steel and heat treatment is different, so it is a better steel comparison than some of the others between different knives. I already have a previous article where I compared CATRA testing to rope cutting so this new test didn’t warrant a whole new article, but I offered an analysis of his test for Patreon. read more

Forging

Forged vs Stock Removal Knives

Thanks to Colin Fergus and funny_name_here for becoming Knife Steel Nerds Patreon supporters!

Forging by the Steel Company vs Bladesmith

When the steel company makes the steel they produce a large melt of the steel with the desired composition and pour it into a mold which solidifies and produces an ingot. A typical ingot size for tool steel or high speed steel might be 10″ thick either round or square depending on the production process and the desired final shape. Smaller ingots are better for limiting the segregation of alloying elements and keeping the cast structure fine. At that point the steel is in “cast” form. The ingot is then heated up to high temperature and forged either with a hammer or press to a form ready for hot rolling. In some cases the ingot is ready for rolling as-produced. Next the steel is hot rolled to the final desired thickness. Hot rolling in an industrial setting is typically done with relatively few reheats, typically single digits. That depends on how much reduction in necessary, how difficult the steel is to work, and the capability of the rolling mill. read more

Carbides, Steel and Knife Properties

Carbide Types in Knife Steels

Thanks to Todd Kroenlein and David for becoming Knife Steel Nerds Patreon supporters!

Cementite

The most basic carbide type in steel is an intermetallic compound formed between iron and carbon, commonly called cementite. Carbides are hard and brittle, similar to a ceramic material. Cementite has a relatively complex structure but in its simplest form it is 3 iron atoms for every carbon atom: Fe3C. However, other elements can partially replace the iron, so the carbide is sometimes given as M3C where M can mean Fe, Mn, Cr, etc. Cementite is typically present as either particles or in “pearlite.” I introduced what pearlite is in this article. However, cementite is the only carbide type that typically forms in pearlite, so to keep things simple for this article I will be focusing on carbide particles. Below I have a schematic representation of carbides (black circles) along with the grain boundaries (black lines). read more

Austempering, Austenitizing, History - Articles - Books

The Secret Heat Treatment of Frank J. Richtig

Thanks to Dean Baughman, Kitoc420, Steve Callari, Jay Ghoo, and Mitch Cagile for becoming Knife Steel Nerds Patreon supporters!

Legendary Heat Treatments

Last week I wrote about What a Good Heat Treatment Can and Cannot Do, and as part of that topic I wrote about how some knifemakers have a legendary or even mythical reputation for their heat treatments. In that article I argued that the big differences are between “bad” and “good” heat treatments, and that the differences between various good heat treatments are much smaller. And that edge geometry and knife design are more important to knife performance than the differences that are possible between different “good” heat treatments. So I think it makes sense to discuss a particular case of a knifemaker known for legendary, unmatched heat treatments, which brings me to… read more

Heat Treating and Processing

What a Good Heat Treatment Can and Cannot Do

Thanks to C6 MFG and Dan Swaney for becoming Knife Steel Nerds Patreon supporters!

The Legend of Heat Treatment

There is some debate about knives that have steel with a “good heat treatment” vs those that have a bad or sub-par heat treatment. Some knifemakers have a near legendary reputation for their excellent heat treatments. What exactly is possible in terms of heat treating? How much better can steel be? How bad can it get? read more