Background
A recent Spyderco Byte has announced a replacement for H1 steel – H2. H1 is known for being a very high corrosion resistance steel used primarily in Spyderco’s Salt line of knives. I have a previous article about the design of H1 and how it “works” which you can read here. I am somewhat tempted to re-write large chunks of that article here because H1 is one of the most misunderstood knife steels but I am going to try to hit a few of the highlights without much explanation and I hope you will read the earlier article to understand what I am referring to: