Category: Heat Treating and Processing
3 thoughts on “Heat Treating and Processing”
Leave a Reply
AR-RPM9 Knife Steel is False Advertising
It gets expensive to buy knives just to cut them up, and metallography costs even more. Support more knife steel research by going to Patreon.com/KnifeSteelNerds You get to read articles and watch videos before anyone else, participate in the Patreon community, and even get a free mug if you sign up for the highest support level.
Testing Chinese Knife Steel 8Cr13MoV/8Cr14MoV
Thank you Patreon Supporters!
Thank you to my Patreon supporters who help make these studies happen. Patreon funds were used for purchasing two ultimately useless knives, and some steel. Patreon supporter Marcus Ho even sent me some steel all the way from China which also ended up not working out. And I used Patreon funds to pay Shawn Houston (also a Patreon supporter) to do microscopy and grind two CATRA knives for me. So when I say that Patreon makes the study happen I don’t mean in an abstract sense. If you want to help fund more knife steel research please come join us on Patreon where you can get articles and videos early. Or if you sign up for the highest tier you can even get a sweet Knife Steel Nerds mug.
USA vs Europe – Powder Metallurgy Knife Steels
Thank you to all the new Knife Steel Nerds Patreon supporters! Your support allows me to do new exciting experiments on knife steel. Some exciting ones coming up in the coming months!
Video
I also have a video which covers the same information (more or less) in this article.
Most Important Property for Knife Steel? Q&A
New Q&A video with questions from Patreon supporters. Go to Patreon.com/KnifeSteelNerds if you want to support knife steel research.
00:00 Ultra high toughness with ferrite/martensite steels?
05:09 Normalize 80CrV2 with stock removal?
How to Heat Treat K390
You can help support more knife steel research like this by going to Patreon.com/KnifeSteelNerds
K390 Steel and Heat Treating Background
I already have a video and article about the history and properties of K390, which you can see here. K390 is a powder metallurgy non-stainless steel with high wear resistance due to very high vanadium, 9%. It is in a similar category to CPM-10V and Vanadis 8.
What is Next After MagnaCut? Q&A Video
New YouTube video is a Q&A from Knife Steel Nerds Patreon supporters. The following topics were covered:
Nitro-V vs 14C28N
Carbide pullout during sharpening
What is difficult about high hardness heat treating of MagnaCut
Damasteel Heat Treatment and Properties
Thanks to the new Knife Steel Nerds Patreon supporters! The newly performed research in this article is all paid for through Patreon funds, such as the purchase of expensive Damasteel. Patreon money is only used for knife steel research. Sara Rempelos, Theo N, Christopher Kuehl, Dirk Hoogenbosch, Nick, nats spawnee, Krisztián Szegi, Todd Ellner, Seth V, Jonathan Graham, Ben Secrist, Drew Certain, Scott Armstuts, Ronald Justin Agee, Jim Darnall, Chris G, Farrell K., Bill Behnke, Paige, Luis Hernandez, clockworkfish, Barry Gordon, KarRawr, Ming Lin, Theodore Loach, Matt Bobchin, Flo, J.T. Pouland, Mark Watt, 愷麒 王, and Nickolay Matershev.
Knife Steel Metallurgist Juha Perttula
Thanks to the new Knife Steel Nerds Patreon supporters! Steve, Bruce Blake, Michael Glaser, James F Khoury, Paul Horner, and Shane Sibert.
Intro
Juha Perttula has a doctorate in metallurgy and he has published several studies in scientific journals on heat treating knife steels. So for this article I want to feature not just an individual study but a person’s work. His studies have focused on traditional bladesmithing, low alloy and carbon steels, and wootz Damascus. He also makes and sells knives which you can read about at his website, juhaperttula.com. Juha’s website also has links to the articles I will be discussing below, and I recommend you read them in addition to my commentary.
How to Heat Treat ApexUltra Knife Steel
Thanks to Windscion, Kalib Maxwell, Jan Ysselstein, Klaas Alberts, Zoltan Gero, Mark Nielsen, Christian Lishen, and Richard Smallwood for becoming Knife Steel Nerds Patreon supporters!
What is ApexUltra?
How to Heat Treat 80CrV2
Thank you to all the new supporters on the Knife Steel Nerds Patreon! This type of research in heat treating wouldn’t be possible without all you supporters. Jim Ballard, Distal Steel, Max Vasilatos, Samuel Hicks, Gundam Iupus, Michael Brauer, Luong La, Chris Hancock, Todd Ellner, Brendon Novak, Yannis Hmade, Kyle Daily, Kenneth Proefrock, JRG, Jason Keen, Robert Johnson, Travis, C. Thomas Guething, Kevin Lavery, Zac War, Justin Smith, Jay Mwangi, Kiyoul Park, Luis Maian, Scott Maslowe, HK Knifeworks, James Hunsberger, Nicholas, Bruce Blake, Matthew Hutchinson, FOBOS Knives, Reiff Knives, Raphael Dall’Anese, Jonathan Shook, Tony Garcia, Dean Paxton, Carey A. Buckles, Pops Knife Supply, J. McConnell, and blank blank.

I consider this site an excellent source for information, I learn something every time I visit.
Have a Bench Made Tagged Out Magna cut. Very tough so far
Ciao Larrin,trovo molto utile questo sito,
Avrei una domanda riguardo all’acciaio A8mod:come é meglio temprarlo per raggiungere la massima durezza?