Super Steel
I see frequent references to “super steel” online, and I was curious about how long that terminology has been around. I did searches on bladeforums as it is one of the oldest knife forums. The number of references to “super steel” has increased over time, but so have the number of posts on bladeforums. I saw how many references to “super steel” there were in each year, and then as a proxy to how many posts there were on bladeforums I did a search for “154” and saw how many references there were each year. Google tops out at 200 results but at that point the dataset was big enough to get an idea: