New Steel and New Patreon Supporters
On Patreon we now have a full set of experiments on the new knife steel I designed for Crucible and Niagara Specialty Metals. The results are extremely promising. Those results are only available on Patreon until it is time to do the formal announcement. Thanks to Chester Dussault, Bob Burland, Matt Masuda, Scott Decker, Philip Dempsey, David Heleander, ConvencienceShout, Chris Pregent, Egan, Morgan Noonan, Michal Galovič, Kumar Muthusamy, Eric Divine, Simon Moeskjær Balle, and Ben Horridge for becoming Knife Steel Nerds Patreon supporters!