Author: Larrin
Cold Forging of Steel
Thanks to Marco Guldimann, Darrin Thomas, Jason Tillostson, Dominic Paolantonio, Ken, Benedikt Peters, and Steve Greiner for becoming Knife Steel Nerds Patreon supporters!
Cold Forging
Cold forging is a lot like hot forging except it is at or near room temperature. The lower temperature means that the steel is much stronger and it is much more difficult to forge. That also means the steel is more brittle and therefore more likely to crack during forging or rolling. The shape of the grains in the steel are changed through forging. You can read about what grains are in this article. Steel is made up of planes of iron atoms, and if the steel was made up of only one grain these planes of atoms would all be parallel to each other:
All About AEB-L
Thanks to anteck7 and Aaron Lee for becoming Knife Steel Nerds Patreon supporters!
History of AEB-L and 13C26
Tracking down the history of AEB-L was surprisingly difficult. The Uddeholm website claims that AEB-L was patented in 1928 [1]; however, that is not entirely truthful. Uddeholm did patent a stainless steel in 1928 [2], which was named AEB, and later AEB-H to differentiate it from AEB-L. This was a very early stainless steel, so its development and patent needs to be viewed in that historical context. You can read about the development of stainless steels in this article. The AEB patent was for 0.7-1.1% carbon, 10-16% chromium, and 0.75-2.0% manganese. The original Brearley and Haynes stainless steel patents were still in effect; they got around them by using a higher carbon content than the Brearley patent (had a 0.7% max), and by claiming that high Mn led to improved corrosion resistance (it actually doesn’t). The nominal composition of AEB became 1% carbon and 13.5% chromium, which gave it a relatively large carbide structure compared to AEB-L, but it did see some use as a razor blade steel.
How Fast Do You Have to Quench? Hardenability of Steel
Thanks to Richard Patterson, Patrick Guignot, Aaron Lee, and David Richardson for becoming Knife Steel Nerds Patreon supporters!
Hardenability
How fast one must quench steel is controlled by its hardenability. Hardenability is not a measure of how hard a steel can get. Instead it is a measure of how fast you have to quench to achieve max hardness for a given composition. Therefore a steel with 0.2% carbon can have high hardenability without being able to reach a particularly high hardness; the steel can be allowed to cool in air and achieve more or less the same hardness as when it is quenched in water. On the other hand, a steel with very high carbon content that can reach very high hardness can have low hardenability, requiring a water quench to achieve its potential hardness.
Niobium-Alloyed Knife Steels – S35VN, S110V, Niolox, and More
Thanks to David Palacios for becoming a Knife Steel Nerds Patreon supporter!
Niobium-Alloyed Steels
Here is a partial list of some niobium-alloyed steels, and I will describe the reasons why the niobium addition was made:
Can CATRA predict Rope Cutting Performance?
Thanks to Fingal Ferguson for becoming a Knife Steel Nerds Patreon supporter!
CATRA Edge Retention Testing
I previously wrote articles about CATRA testing of edges. The CATRA test uses 5% silica-impregnated cardstock which it slices with a fixed stroke length and force. The first article primarily looked at the effect of edge angle on edge retention; specifically, that edge angle greatly controls edge retention:
Book Review – Damascus Steel Swords: Solving the Mystery of How to Make Them
Thanks to Jason Volkert for becoming a Knife Steel Nerds Patreon supporter!
Introduction
In July 2018 a new book was released on the research of wootz Damascus steel by Dr. John Verhoeven. Dr. Verhoeven is well known for his contributions to research on knife steels and damascus, along with frequent collaborator Al Pendray. Dr. Verhoeven has often been cited on this website, including his articles on CATRA testing of different knife steels [1], and also a series of experiments on sharpening of knives [2]. He also wrote a book on the metallurgy of knife steels, which is now published as Steel Metallurgy for the Non-Metallurgist; I reviewed it in this article on book recommendations. Dr. Verhoeven had a particularly strong impact on my interest in steel and metallurgy. I was introduced to him through his knife steel metallurgy book which I read several times in my teen years. And when I was looking for the best steel University to attend, he was the first person I emailed for advice. I asked him for an interview to be published on this website, and he asked if I would be willing to review his new book instead – Damascus Steel Swords: Solving the Mystery of How to Make Them.
History and Properties of 52100 Steel
Thanks to Phil Zhou for becoming a Knife Steel Nerds Patreon supporter! I’ve started posting early test results for things like heat treatment experiments, retained austenite measurements, etc. on Patreon. The data will eventually be posted to this website, but if you want to see it as it comes then get on Patreon.
Does Acidic Food Affect Edge Retention?
Thanks to Bill Wine for becoming a Knife Steel Nerds Patreon supporter!
I was interviewed on the Knife Junkie Podcast, so make sure you check that out.
Acidic Food
Carbon steel knives are frequently used in kitchens, probably the majority of them made by Japanese bladesmiths and knife companies. Kitchen knives cut a variety of foods, and some of them are corrosive. There has been some debate about whether any of these potentially-corrosive foods can actually affect sharpness or edge retention of kitchen knives. Sharpness is controlled by the radius/width of the edge. You can read more in the article on sharpness vs cutting ability.
Which Knife Steels Have the Best Corrosion Resistance?
Thanks to John Scarborough and Robert Angerer for becoming Knife Steel Nerds Patreon supporters!
Update 1/6/2020: I have since performed my own corrosion resistance testing and provided updated analysis.
Knife Steel Nerds 2018 in Review
Here at the beginning of 2019 I decided to write up a retrospective of Knife Steel Nerds so far. A lot of things happened in 2018. First of all, the Knife Steel Nerds website was started, with the first article being posted February 27, 2018. That first article was about a modified 3V steel developed and patented by Crucible but never sold as far as I know. Links to the website were not shared with anyone until March 8th, however.